# Cast iron scrap

Markdown version of https://bluegreenmaterials.com/en/cast-iron-scrap. Updated on 2026-11-20.

Cast iron, which Mexicans call «fierro colado», «fierro vaciado» or «hierro fundido», is an iron alloy with 2 to 4% carbon that is shaped by pouring it into molds[^colado-epa-ap42]. As scrap it is sold separately from steel scrap and has its own grades: cupola cast, engine blocks, broken machinery and borings. Bluegreen buys it lot by lot, makes you an offer within 24 hours after the lot is published and pays you by bank transfer after weighing it.

## Colado, vaciado and fundido: the same material

The RAE dictionary refers «hierro fundido» to «hierro colado»: they are synonyms[^colado-rae-hierro]. UNAM engineering notes call them hierros fundidos, fundiciones de hierro or hierros colados[^colado-unam-fesc]. «Fierro» is how Mexicans say hierro, iron[^fierro-dem], and «vaciar» means forming an object by pouring molten metal into a mold[^colado-dem-vaciar]. That is why fierro colado, fierro vaciado and hierro fundido all name the same scrap: cast iron.

## What cast iron is and how it differs from steel

Cast iron carries 2 to 4% carbon and 0.25 to 3% silicon[^colado-epa-ap42]; steel, less than 2% carbon[^ws-facts]. In gray iron that carbon forms graphite flakes, and each flake acts as a crack: that is why it is brittle[^colado-epa-ap42]. It cannot be rolled or worked hot or cold like steel[^colado-unam-fesc]; parts are made by pouring the metal into molds.

**The types of cast iron[^colado-ucm-atlas]**

| Type | Form of the carbon | How it behaves |
| --- | --- | --- |
| Gray | Graphite flakes, with 1.5 to 3% silicon | The most used in engineering. Its fracture looks gray[^colado-nps-brief27] |
| White | Mostly as iron carbide (cementite) | Very brittle. Its fracture looks white |
| Malleable | Irregular graphite nodules | Made by annealing white iron until the carbide breaks down |
| Ductile or nodular | Graphite spheres, with a little magnesium added before casting | High tensile strength and a silvery look[^colado-epa-ap42] |

## How to tell if a piece is cast iron

- **Gray iron does not bend**: Gray iron is too hard and brittle to be shaped by hammering, rolling or pressing[^colado-nps-brief27]. Ductile and malleable iron do deform somewhat before breaking; if in doubt, choose "Not sure what it is" in the form.
- **It breaks without warning**: Under tension it fails with little warning[^colado-nps-brief27]. That brittleness is what sets it apart from mild steel[^colado-nps-brief27].
- **Gray, grainy fracture**: The broken edge of gray iron looks gray and grainy, which is probably where its name comes from[^colado-nps-brief27].
- **Mold marks**: Cast parts often show mold lines, flashing, casting flaws and air holes, and, unlike wrought iron, they are joined with bolts rather than rivets[^colado-nps-brief27].

## Where cast iron scrap comes from

ReMA's scrap grades name where it comes from: columns, pipe, plates, car and truck engine blocks, parts of farm and other machinery, stoves and grate bars, hammer bases, ingot molds, brake shoes and railroad car wheels[^rema-specs]. Nineteenth century American cities used it widely for water systems and street lighting[^colado-nps-brief27].

A car's engine block counts as cast iron; the body and frame, as [scrap iron](https://bluegreenmaterials.com/en/scrap-iron). Aluminum heads and housings are sold separately, as [aluminum scrap](https://bluegreenmaterials.com/en/aluminum-scrap).

## Cast iron scrap grades

The ReMA (formerly ISRI) specifications circular sorts cast iron by size, cleanliness and origin[^rema-specs]. These are the grades you see most.

**Cast iron grades according to the ReMA circular[^rema-specs]**

| Grade | ReMA code | What it is |
| --- | --- | --- |
| Cupola cast | 252 | Clean cast iron: columns, pipe, plates, engine blocks and machinery parts. Pieces up to 24 by 30 inches and 150 pounds, free of stove plate, burnt iron and brake shoes |
| Mixed cast | 257 | All cast iron grades except burnt iron, to cupola size |
| Heavy breakable cast | 254 | Pieces over charging box size or over 500 pounds that have to be broken |
| Drop broken machinery cast | 261 | Clean heavy cast iron machinery broken under a drop to cupola size |
| Clean auto cast | 259 | Engine blocks free of steel parts (except camshafts, valves, valve springs and studs) and free of nonferrous and non metallic parts |
| Unstripped motor blocks | 260 | Car or truck motors, with or without their steel and nonferrous fittings, free of driveshafts and all frame parts |
| Burnt iron | 256 | Cast iron exposed to fire, such as stove parts and grate bars |
| Malleable | 264 | Malleable iron parts of cars, railroad cars and locomotives, free of cast iron and steel parts |
| Iron borings | 223 | Clean cast or malleable iron borings and drillings, free of steel turnings and excessive oil |

> Any deviation from a grade can be agreed between buyer and seller[^rema-specs]. The steel grades, for the rest of your scrap, are on [scrap iron](https://bluegreenmaterials.com/en/scrap-iron).

## Where it goes: foundries

According to the U.S. EPA, iron foundries melt mainly in cupolas, electric arc furnaces and induction furnaces, and they charge pig iron, iron and steel scrap, foundry returns and turnings; in 1995 it described the cupola as their main furnace[^colado-epa-ap42]. That is why scrap grades ask for pieces «to cupola size».

In the United States, in 2019, iron foundries worked with mixtures that averaged 75% steel scrap[^colado-usgs-myb2019], and the ferrous castings industry consumes most of the scrap the steel mills do not use[^usgs-scrap].

- **587**: metal casting establishments, ferrous and nonferrous, were registered in Mexico in May 2026[^colado-datamexico]
- **109**: of them are in the State of Mexico, the state with the most[^colado-datamexico]
- **95**: are in Nuevo León, and 66 in Jalisco[^colado-datamexico]
- **MXN 51.9 bn**: of gross output came from metal casting in the 2019 Economic Census[^colado-datamexico]

## What lowers the price of your cast iron

- **Steel mixed in.** Cupola cast and clean auto cast do not accept steel parts, except those the circular allows in each grade[^rema-specs].
- **Nonferrous parts.** Clean auto cast must be free of aluminum, copper and non metallic parts[^rema-specs]. Sort them out and sell them separately.
- **Burnt iron and brake shoes.** Cupola cast must come without burnt iron, stove plate or brake shoes[^rema-specs]. Put them in another pile.
- **Size.** Pieces over 24 by 30 inches or over 150 pounds no longer qualify as cupola cast: they are sold in another grade or broken[^rema-specs].
- **Oil.** Borings must come without excessive oil, and clean auto cast is graded differently depending on whether it has been degreased[^rema-specs]. Drain the oil from engines before you sell.

Reference scrap price ranges, with their date, are on [scrap metal prices](https://bluegreenmaterials.com/en/scrap-metal-prices). Payment is calculated from the certified weighbridge weight.

## How to sell your cast iron to Bluegreen

1. **Tell us what you have**: Fill in the form with the type of part, photos and an approximate weight. If you are not sure whether it is cast iron or steel, choose "Not sure what it is" and send photos.
2. **Get the offer**: Once your lot is published, you get an offer within 24 hours. Each lot is assessed on its own.
3. **Pickup**: We collect with our own trucks in any state of Mexico. Projects outside the country are evaluated.
4. **Weighing**: The material is weighed on a certified weighbridge.
5. **Payment and paperwork**: We pay by bank transfer after weighing, never in cash, with a CFDI 4.0 invoice and a Carta Porte 3.1 waybill.

See [how to sell scrap metal step by step](https://bluegreenmaterials.com/en/sell-scrap-metal) and [steel and its scrap](https://bluegreenmaterials.com/en/steel).

## Frequently asked questions

### Are fierro colado and fierro vaciado the same thing?

Yes: both are names for cast iron. The RAE dictionary treats «hierro fundido» and «hierro colado» as synonyms[^colado-rae-hierro].

### How do I tell cast iron from steel?

Gray iron does not bend: it breaks, and its broken edge looks gray and grainy[^colado-nps-brief27]. That brittleness is what sets it apart from mild steel[^colado-nps-brief27]. Ductile and malleable iron deform somewhat before breaking; if in doubt, send photos.

### Do you buy engine blocks?

Yes, as cast iron. Clean, without steel or nonferrous parts, they grade as clean auto cast; complete, as unstripped motor blocks[^rema-specs].

### Is it paid the same as scrap iron?

No. It is quoted separately and has its own grades. See [scrap iron](https://bluegreenmaterials.com/en/scrap-iron) and [scrap metal prices](https://bluegreenmaterials.com/en/scrap-metal-prices).

### Do you buy cast iron borings?

Yes, clean, free of steel turnings and without excessive oil, which is what their grade requires[^rema-specs].

### Do you collect in my state?

Yes. Bluegreen collects with its own trucks in every state of Mexico and evaluates projects outside the country.

### What paperwork comes with the sale?

Every transaction with Bluegreen carries a CFDI 4.0 invoice and a Carta Porte 3.1 waybill, and payment is by bank transfer. See [how the scrap trade is regulated](https://bluegreenmaterials.com/en/regulation).

## Sources

[^colado-epa-ap42]: U.S. Environmental Protection Agency (EPA), «AP-42, Compilation of Air Emissions Factors, Section 12.10: Gray Iron Foundries» (1995). https://www.epa.gov/sites/production/files/2020-11/documents/c12s10.pdf
[^colado-rae-hierro]: Real Academia Española (RAE) y ASALE, «Diccionario de la lengua española, entrada «hierro» (hierro colado, hierro fundido)» (2026). https://dle.rae.es/hierro
[^colado-unam-fesc]: Universidad Nacional Autónoma de México (UNAM), «Lecturas de Ingeniería 3: Hierros fundidos, FES Cuautitlán» (2007). https://virtual.cuautitlan.unam.mx/ingenieriafesc/mecanica/mat/mat_mec/m6/hierro%20fundido.pdf
[^fierro-dem]: El Colegio de México, Diccionario del español de México (DEM), «Diccionario del español de México, entrada «fierro»» (2026). https://dem.colmex.mx/ver/fierro
[^colado-dem-vaciar]: El Colegio de México, Diccionario del español de México (DEM), «Diccionario del español de México, entrada «vaciar»» (2026). https://dem.colmex.mx/ver/vaciar
[^ws-facts]: World Steel Association (worldsteel), «#SteelFacts, June 2026 update» (2026). https://worldsteel.org/wp-content/uploads/SteelFacts_update-June-2026.pdf
[^colado-ucm-atlas]: Universidad Complutense de Madrid (UCM), «Metallographic Atlas: Cast irons» (2026). https://www.ucm.es/metallographicatlas/cast_irons
[^colado-nps-brief27]: U.S. National Park Service (NPS), «Preservation Brief 27: The Maintenance and Repair of Architectural Cast Iron» (1991). https://www.nps.gov/orgs/1739/upload/preservation-brief-27-cast-iron.pdf
[^rema-specs]: Recycled Materials Association (ReMA), «ReMA's ISRI Specifications Circular, Ferrous Scrap Guidelines (FS-2023)» (2026). https://www.isrispecs.org/wp-content/uploads/2026/09/2026-July-ReMA_ISRI_Specifications.pdf
[^colado-usgs-myb2019]: U.S. Geological Survey (USGS), «2019 Minerals Yearbook: Iron and Steel Scrap (advance release)» (2024). https://pubs.usgs.gov/myb/vol1/2019/myb1-2019-iron-steel-scrap.pdf
[^usgs-scrap]: U.S. Geological Survey (USGS), «Mineral Commodity Summaries 2026: Iron and Steel Scrap» (2026). https://pubs.usgs.gov/periodicals/mcs2026/mcs2026-iron-steel-scrap.pdf
[^colado-datamexico]: Secretaría de Economía, Data México, «Data México: Moldeo por fundición de piezas metálicas (SCIAN 3315)» (2026). https://www.economia.gob.mx/datamexico/es/profile/industry/foundries
